Platinum particles deposited on synthetic boron-doped diamond surfaces: application to methanol oxidation
Empreu sempre aquest identificador per citar o enllaçar aquest ítem
http://hdl.handle.net/10045/2704
Títol: | Platinum particles deposited on synthetic boron-doped diamond surfaces: application to methanol oxidation |
---|---|
Autors: | Montilla, Francisco | Morallon, Emilia | Duo, Ilaria | Comninellis, Christos | Vázquez Picó, José Luis |
Grups d'investigació o GITE: | Electrocatálisis y Electroquímica de Polímeros |
Centre, Departament o Servei: | Universidad de Alicante. Departamento de Química Física | Swiss Federal Institute of Technology. Faculty of Basic Science |
Paraules clau: | Diamond electrodes | Electrocatalysis | Platinum catalyst | Electrodeposition | Methanol oxidation |
Àrees de coneixement: | Química Física | Ciencia de Materiales |
Data de creació: | 2002 |
Data de publicació: | 15-de novembre-2003 |
Editor: | Elsevier |
Citació bibliogràfica: | MONTILLA JIMÉNEZ, Francisco, et al. "Platinum particles deposited on synthetic boron-doped diamond surfaces: application to methanol oxidation". Electrochimica Acta. Vol. 48, Issues 25-26 (15 Nov. 2003). ISSN 0013-4686, pp. 3891-3897 |
Resum: | Two methods have been used for the deposition of Pt particles on synthetic boron-doped diamond (BDD) surfaces: chemical deposition and electrodeposition under potentiostatic conditions. However, electrodeposition leads much higher platinum dispersion than chemical deposition. The mechanism of nucleation and growing of the electrodeposited platinum was investigated by means of chronoamperometric studies in acid medium. The electrodeposition on diamond surfaces shows a mechanism of progressive nucleation as deduced from the chronoamperometric studies in acid medium. The stability of the deposited platinum is very low and the platinum particle are dissolved/detached by cycling. The modified BDD electrodes by deposition of platinum have been tested for the oxidation of methanol, showing that multi-step deposition results in higher values of surface and mass activities for methanol oxidation than one-step deposition process. |
Patrocinadors: | Ministerio de Ciencia y Tecnología (MAT2001-1007) |
URI: | http://hdl.handle.net/10045/2704 |
ISSN: | 0013-4686 |
DOI: | 10.1016/S0013-4686(03)00526-7 |
Idioma: | eng |
Tipus: | info:eu-repo/semantics/article |
Revisió científica: | si |
Versió de l'editor: | http://dx.doi.org/10.1016/S0013-4686(03)00526-7 |
Apareix a la col·lecció: | INV - GEPE - Artículos de Revistas |
Arxius per aquest ítem:
Arxiu | Descripció | Tamany | Format | |
---|---|---|---|---|
Electrochimica Acta 48 (2003) 3891-3897.pdf | Versión final (acceso restringido) | 313,51 kB | Adobe PDF | Obrir Sol·licitar una còpia |
Article.pdf | Versión revisada (acceso libre) | 316,25 kB | Adobe PDF | Obrir Vista prèvia |
Tots els documents dipositats a RUA estan protegits per drets d'autors. Alguns drets reservats.